KAIST textures copper foil for anode-free EV batteries

KAIST’s 300-nm copper structures and 10-nm MXene coating seek steadier lithium plating in anode-free cells, though cycle life and factory-scale production remain unproven.

KAIST aims to extend the lifespan of anode-free batteries
KAIST aims to extend the lifespan of anode-free batteriesAlexei_other / pixabay

SPECIFICATION

  1. 1

    KAIST’s structured copper uses tubes about 300 nm wide and 150 nm tall.

  2. 2

    An approximately 10-nm MXene coating helped form a uniform SEI confirmed by spectroscopy and electron microscopy.

  3. 3

    The results appeared in Advanced Functional Materials on September 1.

  4. 4

    A separate November 2025 KAIST-linked cell reached 1,270 Wh/l, retained 81.9% capacity after 100 cycles and averaged 99.6% Coulombic efficiency.

  5. 5

    The new method has no reported energy-density or cycle-stability figures, and industrial scalability remains unresolved.

KAIST researchers equipped copper foil with tubes about 300 nanometers wide and 150 nanometers tall to curb dendrites and extend the life of anode-free batteries. The team, led by professors Jinwoo Lee and Hee-Tae Jung, published its results on September 1 in Advanced Functional Materials.

The project brought KAIST together with Kyungpook National University and South Korea’s National NanoFab Center. Electric Cars Report highlighted the paper and its findings.

What problem does the copper treatment target?

Anode-free cells drop the graphite anode used in conventional lithium-ion batteries. During charging, they deposit lithium directly onto a copper current collector. Removing the anode material reduces cell weight and volume, while the design offers the potential for higher energy density in electric vehicles.

Repeated charging and discharging can make that deposit uneven across the copper. The resulting dendrites—branched lithium structures—speed battery ageing and, in extreme cases, can cause internal short circuits. The lithium-electrolyte boundary layer can also become unstable.

How did KAIST texture the current collector?

Rather than adding lithium or using thicker protective layers, the researchers worked on the current collector’s surface structure. They adapted semiconductor-manufacturing lithography called Secondary Sputtering Lithography (SSL) to form the tubular features.

Compared with conventional smooth copper foil, the treatment provides roughly four times the surface area for lithium deposition. The researchers designed that area to spread lithium more uniformly and counter dendrite formation.

What does the MXene coating change?

They applied an approximately 10-nanometer MXene coating to the structured copper. MXenes are a class of two-dimensional materials; combined with the electrolyte, the coating promotes a lithium-fluoride-rich Solid Electrolyte Interphase, or SEI.

The SEI is intended to reduce unwanted reactions between lithium and electrolyte and inhibit dendrite growth. Spectroscopic and electron microscopic investigations confirmed that a uniform, nanoscale protective layer formed.

Why did the team leave the electrolyte composition alone?

KAIST Professor Jinwoo Lee said: “The advantage of the newly presented method is that it enables uniform lithium deposition and a stable boundary layer without modifying the electrolyte composition or adding excess lithium.” The method therefore leaves the electrolyte formulation unchanged.

The two parts of the treatment target separate failure points. The tubular structures guide where lithium lands, while the MXene-assisted SEI is designed to suppress reactions at the interface. Together, they aim to limit dendrites without excess lithium or a thicker protective layer.

Can the copper collector still trap lithium?

A July study by Ruhr-Universität Bochum, the Helmholtz Institute Ulm and the Karlsruhe Institute of Technology experimentally confirmed another ageing mechanism in lithium-metal batteries. During repeated charging and discharging, lithium penetrates the copper current collector and becomes permanently bound there, reducing available capacity. Whether KAIST’s new treatment also counters this mechanism remains unclear.

What did the earlier KAIST-linked cell achieve?

In November 2025, a separate South Korean team involving KAIST reported these results for an anode-free lithium-metal battery:

  • Volumetric energy density: 1,270 Wh/l
  • Capacity retained after 100 charge cycles: 81.9%
  • Average Coulombic efficiency: 99.6%

According to chemie.de, the 1,270 Wh/l figure was nearly double the volumetric energy density of current lithium-ion batteries for electric vehicles. The earlier cell used a polymer framework with embedded silver nanoparticles to promote uniform deposition, plus a specially developed electrolyte to stabilize the boundary layer; the team also tested pouch cells.

What remains unproven?

The Electric Cars Report account gives no specific energy-density or cycle-stability figures for the new textured copper and MXene combination. It also leaves industrial scalability of the SSL process unresolved; the team still must determine whether the method can reach production levels.

For service departments, the report contains no vehicle application, diagnostic step or repair procedure. The work belongs on the technology watch list until the missing cell data and manufacturing path arrive.

via electrive (Source)

More from Elena Vasquez